Topadd® TIM-810
Description
Acrylic impact modifier is a core-shell type of copolymer consisted of rubbery core (Butyl acrylate) and glass shell which is compatible with PVC, rubbery core transfers the external impact energy into heat and grafted shell provides perfect compatibility of impact modifier with PVC matrix, therefore it shows excellent impact-strength, weather-resistance and color durability under long-period exposure to outdoor conditions.
Advantage:
--Excellent Weatherability: long-term weather resistance and impact and color retention.
--Superior Surface Finish: The wide processing window assures a consistently flawless "satin" surface finish.
--Good Low-Temperature Impact
--Improved Processability: Because of the Low melt viscosity , extrusion temperatures are lower, resulting --in enhanced compound stability and output.
--High Output: The low melt viscosity of allows higher output without increasing extruder amps.
Specification | Unit | Test standard | 810 |
Appearance | -- | -- | White Flowing powder |
Bulk density | g/cm3 | GB/T 1636-2008 | 0.4-0.55 |
Sieve residue (30 mesh) | % | GB/T 2916 | ≤2.0 |
Volatile content | % | ASTM D5668 | ≤1.0 |
Comparison:
ROHM & HAAS : KM-355P
KANEKA : FM-40 , FM-50
Package & Storage
25kg plastic woven bag or 20kg paper bag with PE liner bag.
The product can be stored under appropriate conditions for two years. But please keep products store in a dry ventilated environment (temperature should not exceed 30°C, in low humidity). Especially at high temperatures & high humidity, it is recommended not to stack more than 30 days long, it may increase agglomeration phenomenon. Agglomeration does not affect the quality ,but agglomeration material is smashed before using .
PVC Stabilizer, PVC Processing Aid, PVC Lubricant, PVC Modifier
Product Categories : PVC Modifier > Acrylic Impact Modifier
Home > Products > PVC Modifier > Acrylic Impact Modifier > Modifiers for PVC Pipe
Send Inquiry
Mr. Ron Han
Tel:86-536-8206760
Fax:86-536-8206750
Mobile Phone:+8615336365800
Email:manager.han@novistagroup.com
Address:RM1232-1233,#4 Building No.4778 Shengli East Street, Weifang, Shandong
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.
Fill in more information so that we can get in touch with you faster
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.